  [OT] Melting aluminum Rich <rich@example.invalid> - 2014-09-13 13:07 +0000
    Re: [OT] Melting aluminum Paul Sture <nospam@sture.ch> - 2014-09-13 15:49 +0200
    Re: [OT] Melting aluminum Mike Spencer <mds@bogus.nodomain.nowhere> - 2014-09-13 16:05 -0300
      Re: [OT] Melting aluminum Michael Black <et472@ncf.ca> - 2014-09-13 17:57 -0400
        Re: [OT] Melting aluminum polygonum <rmoudndgers@vrod.co.uk> - 2014-09-13 23:04 +0100
          Re: [OT] Melting aluminum Michael Black <et472@ncf.ca> - 2014-09-14 10:34 -0400
        Re: [OT] Melting aluminum Mike Spencer <mds@bogus.nodomain.nowhere> - 2014-09-13 23:25 -0300

#4869 — [OT] Melting aluminum

FromRich <rich@example.invalid>
Date2014-09-13 13:07 +0000
Subject[OT] Melting aluminum
Message-ID<bqgQpGjuiYlYRWxODIJb+l9w@dont-email.me>
http://ericlippert.com/2014/09/12/melting-aluminum/

   Today another in my ongoing, seldom-updated series of posts about
   building my own backyard foundry. Today I'll describe how the final step
   works: actually melting and pouring the metal. First, see my previous
   post on how to make a green sand mold.

   Start by assembling all the equipment you'll need in one place, on a day
   with no chance of rain. (Click on any photo for a larger version.)

   ...

[toc] | [next] | [standalone]


#4876

FromPaul Sture <nospam@sture.ch>
Date2014-09-13 15:49 +0200
Message-ID<ujudeb-p3t1.ln1@news.chingola.ch>
In reply to#4869
On 2014-09-13, Rich <rich@example.invalid> wrote:
> http://ericlippert.com/2014/09/12/melting-aluminum/
>
>    Today another in my ongoing, seldom-updated series of posts about
>    building my own backyard foundry. Today I'll describe how the final step
>    works: actually melting and pouring the metal. First, see my previous
>    post on how to make a green sand mold.
>
>    Start by assembling all the equipment you'll need in one place, on a day
>    with no chance of rain. (Click on any photo for a larger version.)

Thanks for the link. One of my student holiday jobs was working in an iron
foundry (they made brake blocks for trains) so I got very familiar with
moulding sand.

-- 
People who think they know everything really annoy those of us who know
we don't                                           -- Bjarne Stroustrup

[toc] | [prev] | [next] | [standalone]


#4878

FromMike Spencer <mds@bogus.nodomain.nowhere>
Date2014-09-13 16:05 -0300
Message-ID<87a963ibne.fsf@bogus.nodomain.nowhere>
In reply to#4869
Rich <rich@example.invalid> writes:

> http://ericlippert.com/2014/09/12/melting-aluminum/
> 
>    Today another in my ongoing, seldom-updated series of posts about
>    building my own backyard foundry. Today I'll describe how the final step
>    works: actually melting and pouring the metal. First, see my previous
>    post on how to make a green sand mold.

()()()()

Nice to see another hot-metal head [1] on c.m.  The term "hacker", in its
best sense, isn't limited to digital bits.


[1] Google my name and "blacksmith".

-- 
Mike Spencer                  Nova Scotia, Canada

[toc] | [prev] | [next] | [standalone]


#4883

FromMichael Black <et472@ncf.ca>
Date2014-09-13 17:57 -0400
Message-ID<alpine.LNX.2.02.1409131755550.24400@darkstar.example.org>
In reply to#4878
On Sat, 13 Sep 2014, Mike Spencer wrote:

>
> Rich <rich@example.invalid> writes:
>
>> http://ericlippert.com/2014/09/12/melting-aluminum/
>>
>>    Today another in my ongoing, seldom-updated series of posts about
>>    building my own backyard foundry. Today I'll describe how the final step
>>    works: actually melting and pouring the metal. First, see my previous
>>    post on how to make a green sand mold.
>
> ()()()()
>
> Nice to see another hot-metal head [1] on c.m.  The term "hacker", in its
> best sense, isn't limited to digital bits.
>
>
> [1] Google my name and "blacksmith".
>
But you don't use aluminum do you?

The closest I got to any of this wsa making a screwdriver in metal shop in 
high school forty years ago.  Used a lathe to make the handle, and 
actually heated up the piece of metal for the blade and hammered away, 
then ground some.  A big screwdriver, I still have it, probably becasue 
it's only useful when I need a big screwdriver.

I always liked the notion of making a knife, folding it over again and 
again, then hammering, just like making croissants.

   Michael

[toc] | [prev] | [next] | [standalone]


#4884

Frompolygonum <rmoudndgers@vrod.co.uk>
Date2014-09-13 23:04 +0100
Message-ID<c7jtcdFit7lU1@mid.individual.net>
In reply to#4883
On 13/09/2014 22:57, Michael Black wrote:
>
> I always liked the notion of making a knife, folding it over again and
> again, then hammering, just like making croissants.

Don't think that butter and yeast are often used in knife-making.

-- 
Rod

[toc] | [prev] | [next] | [standalone]


#4895

FromMichael Black <et472@ncf.ca>
Date2014-09-14 10:34 -0400
Message-ID<alpine.LNX.2.02.1409141033550.25472@darkstar.example.org>
In reply to#4884
On Sat, 13 Sep 2014, polygonum wrote:

> On 13/09/2014 22:57, Michael Black wrote:
>> 
>> I always liked the notion of making a knife, folding it over again and
>> again, then hammering, just like making croissants.
>
> Don't think that butter and yeast are often used in knife-making.
>
But in both cases, you want slivers of both layers, so you flatten out, 
and then fold, then faltten again.

   Michael

[toc] | [prev] | [next] | [standalone]


#4886

FromMike Spencer <mds@bogus.nodomain.nowhere>
Date2014-09-13 23:25 -0300
Message-ID<87iokr7xba.fsf@bogus.nodomain.nowhere>
In reply to#4883
Michael Black <et472@ncf.ca> writes:

> On Sat, 13 Sep 2014, Mike Spencer wrote:
> 
>> Rich <rich@example.invalid> writes:
>>
>>> http://ericlippert.com/2014/09/12/melting-aluminum/
>>>
>>
>> Nice to see another hot-metal head [1] on c.m.  The term "hacker", in its
>> best sense, isn't limited to digital bits.
>>
> But you don't use aluminum do you?


Only cold. You can do some nice repousse in Al but it's hard (where I
am) to  find pure Al sheet. The stuff they use for dump trucks and
boat hulls obviously doesn't work for that.

> I always liked the notion of making a knife, folding it over again and 
> again, then hammering...

It's incredibly cool.  In the last 30 years, numerous guys have made
careers specializing in that.  I've made a nice little paring knife,
just to prove I could do it.

> ... just like making croissants.

Almost but not exactly like making croissants, just to be technically
picky.  :-)  Cut and stack, not fold. 

-- 
Mike Spencer                  Nova Scotia, Canada