Groups | Search | Server Info | Keyboard shortcuts | Login | Register [http] [https] [nntp] [nntps]
Groups > sci.engr.joining.welding > #13644
| From | Cydrome Leader <presence@MUNGEpanix.com> |
|---|---|
| Newsgroups | rec.crafts.metalworking, sci.engr.joining.welding |
| Subject | Re: Getting More First Minutes Out of A Flap Disc |
| Date | 2022-05-11 16:56 +0000 |
| Organization | PANIX Public Access Internet and UNIX, NYC |
| Message-ID | <t5gpsa$hhl$1@reader1.panix.com> (permalink) |
| References | <t5gles$nd7$1@gioia.aioe.org> |
Cross-posted to 2 groups.
In rec.crafts.metalworking Bob La Londe <none@none.com99> wrote: > Yesterday I found myself cleaning up a bit of square tube in preparation [boring crap trimmed] So OP wants help finding a better type of flap disc, but never mentions the type they're using now.
Back to sci.engr.joining.welding | Previous | Next — Previous in thread | Next in thread | Find similar
Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-11 08:41 -0700
Re: Getting More First Minutes Out of A Flap Disc David Billington <djb@invalid.com> - 2022-05-11 17:20 +0100
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-11 13:34 -0400
Re: Getting More First Minutes Out of A Flap Disc Clifford Heath <no.spam@please.net> - 2022-05-12 09:39 +1000
Re: Getting More First Minutes Out of A Flap Disc Mike Spencer <mds@bogus.nodomain.nowhere> - 2022-05-12 00:37 -0300
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-12 07:07 -0400
Re: Getting More First Minutes Out of A Flap Disc David Billington <djb@invalid.com> - 2022-05-12 16:03 +0100
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-12 12:04 -0400
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-13 06:52 -0400
Re: Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-11 10:59 -0700
Re: Getting More First Minutes Out of A Flap Disc David Billington <djb@invalid.com> - 2022-05-11 19:05 +0100
Re: Getting More First Minutes Out of A Flap Disc Cydrome Leader <presence@MUNGEpanix.com> - 2022-05-11 16:56 +0000
Re: Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-11 10:08 -0700
Re: Getting More First Minutes Out of A Flap Disc Dirtcrasher <83b08c0a764e217c41bda109411634c3@example.com> - 2023-11-06 04:02 +0000
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-11 13:23 -0400
Re: Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-11 10:58 -0700
Re: Getting More First Minutes Out of A Flap Disc Snag <Snag_one@msn.com> - 2022-05-11 15:30 -0500
Re: Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-11 13:59 -0700
Re: Getting More First Minutes Out of A Flap Disc Snag <Snag_one@msn.com> - 2022-05-11 17:52 -0500
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-11 18:14 -0400
Re: Getting More First Minutes Out of A Flap Disc "Jim Wilkins" <muratlanne@gmail.com> - 2022-05-11 17:30 -0400
Re: Getting More First Minutes Out of A Flap Disc Clifford Heath <no.spam@please.net> - 2022-05-12 09:38 +1000
Re: Getting More First Minutes Out of A Flap Disc Bob Engelhardt <BobEngelhardt@comcast.net> - 2022-05-11 22:29 -0400
Re: Getting More First Minutes Out of A Flap Disc Richard Smith <null@void.com> - 2022-05-12 09:07 +0100
Re: Getting More First Minutes Out of A Flap Disc Dirtcrasher <83b08c0a764e217c41bda109411634c3@example.com> - 2023-11-06 04:02 +0000
Re: Getting More First Minutes Out of A Flap Disc Bob La Londe <none@none.com99> - 2022-05-12 11:30 -0700
csiph-web